Packaging film failures can disrupt production, compromise product protection and increase waste. Understanding their causes helps manufacturers improve material performance and process reliability.

Packaging films must withstand mechanical, thermal and environmental stresses throughout manufacturing, converting, filling, storage and distribution.

Discover B2B Marketing That Performs

Combine business intelligence and editorial excellence to reach engaged professionals across 36 leading media platforms.

Find out more

Yet even materials that perform well in laboratory tests can develop problems under real production conditions. Tearing, puncturing, excessive stretching, wrinkling, poor sealing and inadequate barrier performance can all affect packaging quality and production efficiency.

A film with sufficient tensile strength, for example, may still tear easily from a small notch. Similarly, a material with good oxygen barrier properties may lose its effectiveness if pinholes or cracks develop during converting or handling.

Failures can also arise when a film is poorly matched to the machinery used to process it.

Identifying the underlying causes requires manufacturers to assess the film as part of the complete packaging system, rather than treating material properties and production conditions as separate issues.

Why do packaging films tear or puncture?

Tearing and puncturing are among the most common mechanical failures in flexible packaging.

Tears can develop when films are exposed to excessive tension, sharp edges, poor cutting conditions or repeated mechanical stress. Small defects along a film’s edge can act as starting points for tears, particularly when the material has limited resistance to tear propagation.

Punctures may occur when packaging comes into contact with sharp product features, machinery components or other packages during handling and transport.

Although film thickness influences mechanical performance, it is not the only determining factor.

Polymer selection, molecular orientation, layer structure and processing conditions all affect resistance to tearing and puncturing. A thinner, well-designed multilayer film may outperform a thicker material in a particular application, depending on its construction and the stresses involved.

Manufacturers should assess tensile strength, tear resistance and puncture performance using test methods relevant to the intended application.

Where failures occur repeatedly, corrective measures may include changing the film structure, adjusting machine tension, removing sharp contact points or redesigning the package to reduce localised stress.

How do film thickness and material variations affect performance?

Consistent film properties are essential for reliable converting and packaging operations.

Variations in thickness, commonly known as gauge variation, can affect strength, stiffness, sealing behaviour and how the film travels through machinery.

Thinner areas may be more vulnerable to puncturing or stretching, while thicker sections can contribute to uneven winding and inconsistent sealing conditions.

Differences in polymer composition, additives and layer distribution can also influence performance.

In multilayer films, inconsistent layer thickness may affect barrier properties or mechanical strength, even when the overall film thickness remains within specification.

Manufacturing conditions during extrusion, cooling and orientation can contribute to these variations.

Packaging teams should establish appropriate material specifications and monitor incoming film quality. Thickness measurements, mechanical testing and supplier quality controls can help identify inconsistencies before they cause production problems.

However, specifications should reflect the film’s intended function. Thickness alone is not a reliable measure of overall packaging quality.

Why do films wrinkle, stretch or break on packaging machinery?

Packaging films must travel through rollers, guides, forming equipment and sealing stations while maintaining sufficient dimensional stability.

Problems can develop when web tension, alignment or machine settings are unsuitable for the material.

Excessive tension may stretch or distort the film, while insufficient or uneven tension can contribute to wrinkles, tracking problems and inconsistent feeding.

Misaligned rollers, uneven winding and variations in film stiffness can also affect web handling.

Temperature is another important consideration. Some films become more susceptible to deformation when exposed to heat during processing.

These defects can result in misregistered printing, inaccurate cutting, poor package formation and increased rejection rates.

Preventing web-handling problems requires manufacturers to match machine settings to the film’s mechanical and thermal characteristics.

Tension, roller alignment, unwind conditions and operating speeds should be monitored, particularly when introducing a new film structure or reducing material thickness.

Production trials under representative operating conditions can reveal handling problems that may not be apparent from material specifications or laboratory testing.

Why do packaging film seals fail?

Heat seals are often among the most vulnerable parts of a flexible package.

Failures can occur when the film’s sealant layer is incompatible with the sealing process or when operating conditions fall outside the effective sealing window.

Temperature, pressure and dwell time all influence how sealant layers bond.

Insufficient heat or dwell time may produce weak seals, while excessive heat can distort or damage the film.

Contamination from product residues, moisture, oils or powders can interfere with sealing and create channels through which air or liquids may escape. Film wrinkles and poor alignment can also prevent consistent contact between sealing surfaces.

Manufacturers should distinguish between seal strength and package integrity.

A seal may withstand a mechanical strength test yet still contain a small leak. Conversely, a leak-tight seal may not have sufficient strength to withstand handling and transport.

Seal-strength, leak and hot-tack testing can help identify weaknesses, depending on the packaging application.

Prevention involves selecting suitable sealant materials, establishing a reliable sealing window and controlling contamination, alignment and machine settings.

How do packaging films lose their barrier properties?

Many packaging films are designed to restrict the movement of oxygen, moisture and other substances that can affect product quality and shelf life.

Barrier performance depends on polymer selection, film thickness, multilayer construction and any coatings or metallised layers used.

However, a film’s measured barrier properties do not necessarily reflect the protection delivered by the finished package.

Pinholes, flex cracks, damaged coatings and poor seals can create pathways through which oxygen or moisture can enter.

Repeated bending and mechanical stress are particularly important for structures containing relatively brittle barrier layers.

Environmental conditions can also influence performance. For example, the oxygen barrier properties of ethylene vinyl alcohol (EVOH) can deteriorate under high-humidity conditions.

Oxygen transmission rate (OTR) and water vapour transmission rate (WVTR) testing help manufacturers assess barrier performance under defined conditions.

Where mechanical damage is a concern, testing should also examine the film after representative flexing, handling and distribution stresses.

Finished-package integrity assessments and product shelf-life studies provide further evidence of whether the packaging delivers the required protection.

Can storage and handling damage packaging films?

Packaging films can become damaged or deteriorate before they reach the filling line.

Poor storage conditions, excessive heat, direct sunlight and unsuitable humidity can affect certain materials, coatings and adhesives.

Film rolls may also suffer damage through incorrect stacking, rough handling or excessive pressure.

Deformed roll cores, damaged edges and uneven winding can create problems during unwinding and converting.

For laminated films, insufficient adhesive curing or unsuitable storage conditions may contribute to bonding problems.

Manufacturers should follow material-specific storage requirements and protect rolls from physical damage and environmental exposure.

Incoming inspections can identify visible defects, while appropriate stock rotation and traceability help ensure materials remain suitable for use.

Storage controls should reflect the characteristics of each film rather than assuming that all flexible packaging materials respond to environmental conditions in the same way.

How can testing identify film weaknesses before production?

Testing helps manufacturers determine whether a film is suitable for its intended application before committing to commercial production.

Mechanical assessments may include tensile strength, elongation, tear resistance, puncture resistance and impact performance.

Seal-strength and leak testing can assess closure performance, while OTR and WVTR measurements help evaluate barrier properties.

For laminated structures, bond-strength testing may also be necessary to assess the integrity of individual layers.

Recognised ASTM and ISO test methods provide consistent procedures, although the appropriate method and acceptance criteria depend on the material and application.

Laboratory results should be supported by production trials using representative films, machine settings and packaging formats.

These trials can reveal problems involving web handling, sealing, forming and cutting that may not emerge during isolated material tests.

Testing finished packages after simulated distribution can also help identify failures caused by repeated handling, compression or flexing.

The objective is to verify performance under realistic operating conditions rather than relying on a single laboratory measurement.

How can manufacturers prevent recurring film failures?

Preventing recurring defects requires a structured approach to identifying their underlying causes.

The first step is to establish whether failures originate during film manufacture, converting, filling, storage or distribution.

Production records, material specifications, inspection results and operator observations can help narrow down the possible causes.

For example, repeated tearing at the same point on a packaging line may indicate excessive tension or a sharp machine component rather than inadequate film strength.

Seal defects that appear only at higher production speeds may suggest that the available sealing time is insufficient.

Barrier failures following transport may point to flex cracking or package damage rather than inadequate initial barrier properties.

Corrective actions should target the identified cause and be verified through appropriate testing.

These may include changes to film construction, improved process control, machinery adjustments, revised handling procedures or tighter material specifications.

Manufacturers should also consider whether changes introduced to resolve one problem could create another. Increasing stiffness, for example, may improve handling on some equipment but adversely affect folding or puncture performance.

Improving packaging film performance across the supply chain

Packaging film reliability depends on more than material strength or thickness.

A successful film must withstand converting and filling operations, form reliable seals, maintain its protective properties and survive storage and distribution.

Problems often arise when materials are assessed in isolation rather than as part of the complete packaging system.

By combining appropriate material selection, consistent manufacturing quality, controlled processing conditions and representative performance testing, manufacturers can identify weaknesses before they develop into recurring production defects.

The objective is not simply to make packaging films stronger or thicker. It is to ensure they deliver the required protection and processing performance while minimising waste, maintaining production efficiency and safeguarding product quality.